SABIC Innovative Plastics CYCOLOY LG9000 ABS + Polycarbonate (North America)


Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

Physical PropertiesOriginal ValueComments
Density1.13 g/cc ASTM D 792
Water Absorption0.1 % 24 hours @ 73F; ASTM D 570
Water Absorption at Saturation0.4 % Equilibrium, 73F; ASTM D 570
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.005 - 0.007 cm/cm 0.125 inch; ASTM D 955
Melt Flow17 g/10 min 260C/5.0 kgf; ASTM D 1238

Mechanical Properties
Hardness, Rockwell R118 ASTM D 785
Tensile Strength @ Yield7900 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break75 % Type I, 2.0 in/min; ASTM D 638
Flexural Modulus335000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength12300 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Notched, Low Temp6 ft-lb/in at -22F; ASTM D 256
Gardner Impact @ 23°C300 in-lb Instrumented Impact Total Energy, -22F; ASTM D 3763
Gardner Impact @ 23°C360 in-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched10 ft-lb/in 73F; ASTM D 256

Electrical Properties
Arc Resistance60 - 120 sec Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495
Comparative Tracking Index250 - 400 V (+/- 0.125 inch); PLC Code 2; UL 746A
Hot Wire Ignition, HWI30 - 60 sec (+/- 0.125 inch); PLC Code 2; UL 746A
High Amp Arc Ignition, HAIMin 120 arcs Surface (+/- 0.125 inch); PLC Code 0; UL 746A

Thermal Properties
CTE, linear, 212°F (100°C)40 µin/in-°F Cross Flow; 0F to 300F; ASTM E 831
CTE, linear, 212°F (100°C)40 µin/in-°F Flow, 0F to 300F; ASTM E 831
Thermal Conductivity0.2 W/m-K ASTM C 177
Deflection Temperature at 0.46 MPa (66 psi)255 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 0.46 MPa (66 psi)265 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)225 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)230 °F 0.250 inch, unannealed; ASTM D 648
Vicat Softening Point265 °F Rate B; ASTM D 1525
UL RTI, Electrical60 °C UL 746B
UL RTI, Mechanical with Impact60 °C UL 746B
UL RTI, Mechanical without Impact60 °C UL 746B
Flammability, UL94HB 0.059 in.

Optical Properties
Gloss30 % Untextured, 60 degrees; ASTM D 523

Descriptive Properties
CSA File No.LS88480 
UL File Number, USAE121562 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.