MatWeb, The Online Materials Database
SABIC Innovative Plastics CYCOLOY MC8100 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.13 g/cc | ASTM D 792 |
| Water Absorption | 0.1 % | 24 hours @ 73F; ASTM D 570 |
| Water Absorption at Saturation | 0.4 % | Equilibrium, 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.004 - 0.007 cm/cm | Flow, 0.125 inch; ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 7600 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 100 % | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Yield | 5 % | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Modulus | 300000 psi | 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 300000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Yield Strength | 11200 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Notched, Low Temp | 8 ft-lb/in | at -22F; ASTM D 256 |
| Gardner Impact @ 23°C | 420 in-lb | Instrumented Impact Total Energy, -22F; ASTM D 3763 |
| Gardner Impact @ 23°C | 480 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
| Izod Impact, Notched | 10 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
| CTE, linear 68°F | 45 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
| Thermal Conductivity | 0.2 W/m-K | ASTM C 177 |
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °F | 0.125 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 220 °F | 0.125 inch, unannealed; ASTM D 648 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |