SABIC Innovative Plastics CYCOLOY MC9000 ABS + Polycarbonate (North America)
Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.14 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Melt Flow | 22 g/10 min | 260C/5.0 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 8600 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 75 % | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Yield | 5 % | Type I, 2.0 in/min; ASTM D 638 |
| Tensile Modulus | 320000 psi | 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 345000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Yield Strength | 12600 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Notched, Low Temp | 5 ft-lb/in | at -22F; ASTM D 256 |
| Gardner Impact @ 23°C | 520 in-lb | Instrumented Impact Total Energy, -22F; ASTM D 3763 |
| Gardner Impact @ 23°C | 540 in-lb | Instrumented Impact Total Energy, 73°F; ASTM D 3763 |
| Izod Impact, Notched | 12 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
| CTE, linear 68°F | 40 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 260 °F | 0.125 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 230 °F | 0.125 inch, unannealed; ASTM D 648 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |