MatWeb, The Online Materials Database
SABIC Innovative Plastics ULTEM ATX100 Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.21 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Melt Flow | 6 g/10 min | 295C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 10000 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 80 % | Type I, 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 368000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 15500 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Unnotched | 39 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 8 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Comparative Tracking Index | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
| Hot Wire Ignition, HWI | 60 - 120 sec | (+/- 0.125 inch); PLC Code 1; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 315 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 115 °C | UL 746B |
| UL RTI, Mechanical with Impact | 115 °C | UL 746B |
| UL RTI, Mechanical without Impact | 115 °C | UL 746B |
| Flammability, UL94 | HB | 0.03 in. |
Descriptive Properties | |
| CSA File No. | LS88480 | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of