MatWeb, The Online Materials Database
SABIC Innovative Plastics ULTEM CRS5111 Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.36 g/cc | ASTM D 792 |
| Melt Flow | 6.9 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Break | 16300 psi | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Strength @ Yield | 17000 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 4 % | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Modulus | 690000 psi | 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 710000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 28000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Notched | 0.7 ft-lb/in | 73F; ASTM D 256 |
| Izod Impact, Notched | 6.7 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | 120 - 180 sec | Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495 |
| Comparative Tracking Index | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
| Hot Wire Ignition, HWI | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Amp Arc Ignition, HAI | Max 15 arcs | Surface (+/- 0.125 inch); PLC Code 4; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 420 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 105 °C | UL 746B |
| UL RTI, Mechanical with Impact | 105 °C | UL 746B |
| UL RTI, Mechanical without Impact | 105 °C | UL 746B |
| Flammability, UL94 | V-0 | 0.058 in. |
| Flammability, UL94 | 7 | 0.058 in. |
Descriptive Properties | |
| CSA File No. | LS88480 | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |