Physical PropertiesOriginal ValueComments
Density1.51 g/cc ASTM D 792
Linear Mold Shrinkage0.002 - 0.004 cm/cm Flow, 0.125 inch; ASTM D 955
Melt Flow1.8 g/10 min 337C/6.6 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Break24000 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break3 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus1.3e+006 psi 0.2 in/min; ASTM D 638
Flexural Modulus1.3e+006 psi 0.10 in/min, 4" span; ASTM D 790
Flexural Yield Strength34000 psi 0.10 in/min, 4" span; ASTM D 790
Izod Impact, Notched10.4 ft-lb/in Reverse Notched, 73F; ASTM D 256
Izod Impact, Notched2.1 ft-lb/in 73F; ASTM D 256

Electrical Properties
Arc Resistance120 - 180 sec Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495
Comparative Tracking Index100 - 175 V (+/- 0.125 inch); PLC Code 4; UL 746A
Hot Wire Ignition, HWI30 - 60 sec (+/- 0.125 inch); PLC Code 2; UL 746A
High Amp Arc Ignition, HAIMax 15 arcs Surface (+/- 0.125 inch); PLC Code 4; UL 746A
High Voltage Arc-Tracking Rate, HVTRMin 150 mm/min (+/- 0.125 inch); PLC Code 4; UL 746A

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)430 °F 0.250 inch, unannealed; ASTM D 648
UL RTI, Electrical105 °C UL 746B
UL RTI, Mechanical with Impact105 °C UL 746B
UL RTI, Mechanical without Impact105 °C UL 746B
Flammability, UL94V-0 0.058 in.
Flammability, UL947 0.058 in.

Descriptive Properties
CSA File No.LS88480 
UL File Number, USAE121562 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.