MatWeb, The Online Materials Database

SABIC Innovative Plastics ULTEM CRS5311 Polyetherimide (North America)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

Physical PropertiesMetricEnglishComments
Density1.52 g/cc0.0549 lb/in³ ASTM D 792
Linear Mold Shrinkage0.002 - 0.004 cm/cm0.002 - 0.004 in/in Flow, 0.125 inch; ASTM D 955
Melt Flow4 g/10 min4 g/10 min 337C/6.6 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Break165 MPa24000 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break3 %3 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus8.96 GPa1300 ksi 0.2 in/min; ASTM D 638
Flexural Modulus8.96 GPa1300 ksi 0.10 in/min, 4" span; ASTM D 790
Flexural Yield Strength234 MPa34000 psi 0.10 in/min, 4" span; ASTM D 790
Izod Impact, Notched0.961 J/cm1.8 ft-lb/in 73F; ASTM D 256
Izod Impact, Notched1.6 J/cm3 ft-lb/in Natural, tints; ASTM D 256
Izod Impact, Notched5.07 J/cm9.5 ft-lb/in Reverse Notched, 73F; ASTM D 256

Electrical Properties
Arc Resistance120 - 180 sec120 - 180 sec Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495
Comparative Tracking Index100 - 175 V100 - 175 V (+/- 0.125 inch); PLC Code 4; UL 746A
Hot Wire Ignition, HWIMin 120 secMin 120 sec (+/- 0.125 inch); PLC Code 0; UL 746A
High Amp Arc Ignition, HAIMax 15 arcsMax 15 arcs Surface (+/- 0.125 inch); PLC Code 4; UL 746A
High Voltage Arc-Tracking Rate, HVTR80 - 150 mm/min3.15 - 5.91 in/min (+/- 0.125 inch); PLC Code 3; UL 746A

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)219 °C426 °F 0.250 inch, unannealed; ASTM D 648
UL RTI, Electrical105 °C221 °F UL 746B
UL RTI, Mechanical with Impact105 °C221 °F UL 746B
UL RTI, Mechanical without Impact105 °C221 °F UL 746B
Flammability, UL94V-0V-0 0.058 in.
Flammability, UL9477 0.058 in.

Descriptive Properties
CSA File No.LS88480 
UL File Number, USAE121562 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.