Physical PropertiesMetricEnglishComments
Density1.36 g/cc0.0491 lb/in³ ASTM D 792
Linear Mold Shrinkage0.005 - 0.007 cm/cm0.005 - 0.007 in/in Flow, 0.125 inch; ASTM D 955
Melt Flow16 g/10 min16 g/10 min 337C/6.6 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Yield110 MPa16000 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break70 %70 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus3.72 GPa540 ksi 0.2 in/min; ASTM D 638
Flexural Modulus3.72 GPa540 ksi 0.10 in/min, 4" span; ASTM D 790
Flexural Yield Strength165 MPa24000 psi 0.10 in/min, 4" span; ASTM D 790
Gardner Impact23 J17 ft-lb 73F; ASTM D 3029
Izod Impact, Notched16 J/cm30 ft-lb/in Reverse Notched, 73F; ASTM D 256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)199 °C390 °F 0.250 inch, unannealed; ASTM D 648

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.