| Physical Properties | Metric | English | Comments |
|
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D 792 |
| Melt Flow | 8.4 g/10 min | 8.4 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Hardness, Rockwell M | 114 | 114 | ASTM D 785 |
| Tensile Strength @ Break | 140 MPa | 20300 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 4 % | 4 % | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Modulus | 6.89 GPa | 1000 ksi | 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 6.89 GPa | 1000 ksi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Strength | 228 MPa | 33000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Unnotched | 4.75 J/cm | 8.9 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 0.641 J/cm | 1.2 ft-lb/in | 73F; ASTM D 256 |
| Izod Impact, Notched | 4.54 J/cm | 8.5 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
| Comparative Tracking Index | 100 - 175 V | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | (+/- 0.125 inch); PLC Code 1; UL 746A |
| High Amp Arc Ignition, HAI | Max 15 arcs | Max 15 arcs | Surface (+/- 0.125 inch); PLC Code 4; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 80 mm/min | 1 - 3.15 in/min | (+/- 0.125 inch); PLC Code 2; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 211 °C | 412 °F | 0.250 inch, unannealed; ASTM D 648 |
| Vicat Softening Point | 226 °C | 438 °F | Rate B; ASTM D 1525 |
| UL RTI, Electrical | 170 °C | 338 °F | UL 746B |
| UL RTI, Mechanical with Impact | 170 °C | 338 °F | UL 746B |
| UL RTI, Mechanical without Impact | 170 °C | 338 °F | UL 746B |
| Flammability, UL94 | V-0 | V-0 | 0.016 in. |
| Flammability, UL94 | 7 | 7 | 0.075 in. |
| NBS Smoke Density | 1.3 | 1.3 | Flaming, Ds 4 min; ASTM E 662 |
| NBS Smoke Density | 27 | 27 | Flaming, Dmax 20 min; ASTM E 662 |
| Oxygen Index | 50 % | 50 % | ASTM D 2863 |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |