MatWeb, The Online Materials Database

SABIC Innovative Plastics ULTEM 2212EPR Polyetherimide (North America)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesOriginal ValueComments
Density1.4 g/cc ASTM D 792
Linear Mold Shrinkage0.005 - 0.007 cm/cm Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.005 - 0.007 cm/cm 0.125 inch; ASTM D 955
Melt Flow15 g/10 min 337C/6.6 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Break15600 psi Type I, 0.2 in/min; ASTM D 638
Tensile Strength @ Yield15600 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break3 % Type I, 0.2 in/min; ASTM D 638
Elongation at Yield3 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus840000 psi 0.2 in/min; ASTM D 638
Flexural Modulus740000 psi 0.10 in/min, 4" span; ASTM D 790
Flexural Modulus800000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Strength25000 psi 0.10 in/min, 4" span; ASTM D 790
Flexural Yield Strength25000 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Unnotched9 ft-lb/in 73F; ASTM D 4812
Gardner Impact @ 23°C108 in-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched1.1 ft-lb/in 73F; ASTM D 256

Electrical Properties
Arc Resistance120 - 180 sec Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495
Comparative Tracking Index100 - 175 V (+/- 0.125 inch); PLC Code 4; UL 746A
Hot Wire Ignition, HWI60 - 120 sec (+/- 0.125 inch); PLC Code 1; UL 746A
High Amp Arc Ignition, HAIMax 15 arcs Surface (+/- 0.125 inch); PLC Code 4; UL 746A
High Voltage Arc-Tracking Rate, HVTRMin 150 mm/min (+/- 0.125 inch); PLC Code 4; UL 746A

Thermal Properties
CTE, linear 68°F20 µin/in-°F Flow, -40F to 100F; ASTM E 831
CTE, linear 68°F, Transverse to Flow40 µin/in-°F from -40F to 100F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)410 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 0.46 MPa (66 psi)415 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)401 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)405 °F 0.250 inch, unannealed; ASTM D 648
Vicat Softening Point410 °F Rate B; ASTM D 1525
UL RTI, Electrical105 °C UL 746B
UL RTI, Mechanical with Impact105 °C UL 746B
UL RTI, Mechanical without Impact105 °C UL 746B
Flammability, UL94V-0 0.016 in.

Descriptive Properties
UL File Number, USAE121562 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.