| Physical Properties | Metric | English | Comments |
|
| Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D 792 |
| Linear Mold Shrinkage | 0.002 - 0.004 cm/cm | 0.002 - 0.004 in/in | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.002 - 0.004 cm/cm | 0.002 - 0.004 in/in | 0.125 inch; ASTM D 955 |
| Melt Flow | 7.6 g/10 min | 7.6 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Break | 159 MPa | 23000 psi | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Strength @ Yield | 169 MPa | 24500 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 2 % | 2 % | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Modulus | 9.24 GPa | 1340 ksi | 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 9.24 GPa | 1340 ksi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Strength | 221 MPa | 32000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Notched | 0.854 J/cm | 1.6 ft-lb/in | 73F; ASTM D 256 |
| Izod Impact, Notched | 4.38 J/cm | 8.2 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
| Comparative Tracking Index | 100 - 175 V | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | (+/- 0.125 inch); PLC Code 1; UL 746A |
| High Amp Arc Ignition, HAI | Max 15 arcs | Max 15 arcs | Surface (+/- 0.125 inch); PLC Code 4; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | 3.15 - 5.91 in/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
| CTE, linear, 212°F (100°C) | 41.4 µm/m-°C | 23 µin/in-°F | Cross Flow; 0F to 300F; ASTM E 831 |
| CTE, linear, 212°F (100°C) | 16.2 µm/m-°C | 9 µin/in-°F | Flow, 0F to 300F; ASTM E 831 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 180 °C | 356 °F | UL 746B |
| UL RTI, Mechanical with Impact | 170 °C | 338 °F | UL 746B |
| UL RTI, Mechanical without Impact | 180 °C | 356 °F | UL 746B |
| Flammability, UL94 | V-0 | V-0 | 0.01 in. |
| Flammability, UL94 | 7 | 7 | 0.048 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |