SABIC Innovative Plastics ULTEM 4000 Polyetherimide (North America)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Original Value | Comments |
|
| Density | 1.67 g/cc | ASTM D 792 |
| Water Absorption | 0.11 % | 24 hours @ 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.002 - 0.003 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Melt Flow | 3.1 g/10 min | 337C/6.6 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Hardness, Rockwell M | 85 | ASTM D 785 |
| Tensile Strength @ Break | 12000 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 1.2 % | Type I, 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 1.28e+006 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Strength | 20000 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Flexural Yield Strength | 16500 psi | 0.10 in/min, 4" span; ASTM D 790 |
| Izod Impact, Unnotched | 3 ft-lb/in | 73F; ASTM D 4812 |
| Coefficient of Friction | 0.24 | Vs. Steel, Kinetic; ASTM D 1894 |
| Coefficient of Friction, Static | 0.25 | Vs. Steel; ASTM D 1894 |
| K (wear) Factor | 1900 x 10-10 in³-min/ft-lb-hr | PV=2000 psi-fpm vs Self; GE Test |
| K (wear) Factor | 62 x 10-10 in³-min/ft-lb-hr | PV = 2000 psi-fpm vs Steel; GE Test |
| Limiting Pressure Velocity | 60000 psi-ft/min | 100 fpm; GE Test |
| Taber Abrasion, mg/1000 Cycles | 33 | CS-17, 1 kg; ASTM D 1044 |
| Izod Impact, Notched | 1.2 ft-lb/in | 73F; ASTM D 256 |
| Izod Impact, Notched | 3.2 ft-lb/in | Reverse Notched, 73F; ASTM D 256 |
Electrical Properties |
|
| Comparative Tracking Index | 100 - 175 V | (+/- 0.125 inch); PLC Code 4; UL 746A |
Thermal Properties |
|
| CTE, linear 68°F | 9 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
| CTE, linear, 212°F (100°C) | 9 µin/in-°F | Flow, 0F to 300F; ASTM E 831 |
| Deflection Temperature at 1.8 MPa (264 psi) | 414 °F | 0.250 inch, unannealed; ASTM D 648 |
| Vicat Softening Point | 453 °F | Rate B; ASTM D 1525 |
| UL RTI, Electrical | 105 °C | UL 746B |
| UL RTI, Mechanical with Impact | 105 °C | UL 746B |
| UL RTI, Mechanical without Impact | 105 °C | UL 746B |
| Flammability, UL94 | V-0 | 0.033 in. |
Descriptive Properties | |
| UL File Number, GLOBAL | E161759 | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |