SABIC Innovative Plastics ULTEM 4211 Polyetherimide (North America)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesMetricEnglishComments
Density1.48 g/cc0.0535 lb/in³ ASTM D 792
Melt Flow10.3 g/10 min10.3 g/10 min 337C/6.6 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Yield129 MPa18750 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break3 %3 % Type I, 0.2 in/min; ASTM D 638
Flexural Modulus7.1 GPa1030 ksi 0.10 in/min, 4" span; ASTM D 790
Flexural Strength193 MPa28000 psi 0.10 in/min, 4" span; ASTM D 790
Izod Impact, Notched4.38 J/cm8.2 ft-lb/in Reverse Notched, 73F; ASTM D 256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)212 °C414 °F 0.250 inch, unannealed; ASTM D 648

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.