MatWeb, The Online Materials Database

SABIC Innovative Plastics ULTEM 8015 Polyetherimide (North America)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesOriginal ValueComments
Density1.29 g/cc ASTM D 792
Linear Mold Shrinkage0.004 - 0.005 cm/cm Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.006 - 0.008 cm/cm 0.125 inch; ASTM D 955
Melt Flow2.7 g/10 min 295C/6.6 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Break13000 psi Type I, 0.2 in/min; ASTM D 638
Tensile Strength @ Yield14000 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break80 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus480000 psi 0.2 in/min; ASTM D 638
Flexural Modulus460000 psi 0.10 in/min, 4" span; ASTM D 790
Flexural Yield Strength21000 psi 0.10 in/min, 4" span; ASTM D 790
Gardner Impact @ 23°C500 in-lb Instrumented Impact Energy @ peak, -22°F; ASTM D 3763
Gardner Impact @ 23°C635 in-lb Instrumented Impact Energy @ peak, 73°F; ASTM D 3763
Izod Impact, Notched1.2 ft-lb/in 73F; ASTM D 256
Izod Impact, Notched39 ft-lb/in Reverse Notched, 73F; ASTM D 256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)370 °F 0.250 inch, unannealed; ASTM D 648
Flammability Test45 OSU 2 minute heat, release rate; KW-Min/m2; FAR 25.853
Flammability Test5 Vertical Burn, length; inches; FAR 25.853
Flammability Test80 OSU Peak Heat Release Rate (horizontal); KW/m2; FAR 25.853

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.