SABIC Innovative Plastics ULTEM 9075 Polyetherimide (North America)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.

Physical PropertiesMetricEnglishComments
Density1.3 g/cc0.047 lb/in³ ASTM D 792
Halogen Content0 %0 % GE Test
Linear Mold Shrinkage0.005 - 0.007 cm/cm0.005 - 0.007 in/in Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.005 - 0.007 cm/cm0.005 - 0.007 in/in 0.125 inch; ASTM D 955
Melt Flow2.4 g/10 min2.4 g/10 min 295C/6.6 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Yield96.5 MPa14000 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break85 %85 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus3.31 GPa480 ksi 0.2 in/min; ASTM D 638
Flexural Modulus3.24 GPa470 ksi 0.10 in/min, 4" span; ASTM D 790
Flexural Strength141 MPa20500 psi 0.10 in/min, 4" span; ASTM D 790
Flexural Yield Strength145 MPa21000 psi 0.10 in/min, 4" span; ASTM D 790
Gardner Impact35.3 J26 ft-lb 73F; ASTM D 3029
Izod Impact, Notched0.694 J/cm1.3 ft-lb/in 73F; ASTM D 256
Izod Impact, Notched20.8 J/cm39 ft-lb/in Reverse Notched, 73F; ASTM D 256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)189 °C372 °F 0.250 inch, unannealed; ASTM D 648
Flammability Test00 Vertical Burn, drip time; seconds; FAR 25.853
Flammability Test11 Vertical Burn, extinguish time; seconds; FAR 25.853
Flammability Test1010 OSU 2 minute heat, release rate; KW-Min/m2; FAR 25.853
Flammability Test55 Vertical Burn, length; inches; FAR 25.853
NBS Smoke Density55 Flaming, Dmax; FAR 25.853

Descriptive Properties
FAR 25.853SECT A-1 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.