Physical PropertiesMetricEnglishComments
Density1.73 g/cc0.0625 lb/in³ ASTM D 792
Linear Mold Shrinkage0.002 - 0.003 cm/cm0.002 - 0.003 in/in Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.005 - 0.006 cm/cm0.005 - 0.006 in/in 0.125 inch; ASTM D 955
Melt Flow45 g/10 min45 g/10 min 266C/5.0 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Break110 MPa16000 psi Type I, 0.2 in/min; ASTM D 638
Tensile Strength @ Yield108 MPa15700 psi Type I, 0.2 in/min; ASTM D 638
Elongation at Break3.1 %3.1 % Type I, 0.2 in/min; ASTM D 638
Tensile Modulus6.21 GPa900 ksi 0.2 in/min; ASTM D 638
Flexural Modulus8.27 GPa1200 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Strength155 MPa22500 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Unnotched5.34 J/cm10 ft-lb/in 73F; ASTM D 4812
Izod Impact, Notched0.801 J/cm1.5 ft-lb/in 73F; ASTM D 256

Electrical Properties
Arc Resistance120 - 180 sec120 - 180 sec Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495
Comparative Tracking Index175 - 250 V175 - 250 V (+/- 0.125 inch); PLC Code 3; UL 746A
Hot Wire Ignition, HWIMin 120 secMin 120 sec (+/- 0.125 inch); PLC Code 0; UL 746A
High Amp Arc Ignition, HAIMin 120 arcsMin 120 arcs Surface (+/- 0.125 inch); PLC Code 0; UL 746A
High Voltage Arc-Tracking Rate, HVTRMin 150 mm/minMin 5.91 in/min (+/- 0.125 inch); PLC Code 4; UL 746A

Thermal Properties
Deflection Temperature at 0.46 MPa (66 psi)213 °C415 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)188 °C370 °F 0.250 inch, unannealed; ASTM D 648
UL RTI, Electrical130 °C266 °F UL 746B
UL RTI, Mechanical with Impact130 °C266 °F UL 746B
UL RTI, Mechanical without Impact140 °C284 °F UL 746B
Flammability, UL94V-0V-0 0.03 in.
Flammability, UL9477 0.118 in.

Descriptive Properties
UL File Number, USAE121562 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.