SABIC Innovative Plastics VALOX CS860 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.73 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.002 - 0.003 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.005 - 0.006 cm/cm | 0.125 inch; ASTM D 955 |
| Melt Flow | 45 g/10 min | 266C/5.0 kgf; ASTM D 1238 |
Mechanical Properties |
|
| Tensile Strength @ Break | 16000 psi | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Strength @ Yield | 15700 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 3.1 % | Type I, 0.2 in/min; ASTM D 638 |
| Tensile Modulus | 900000 psi | 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 1.2e+006 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Strength | 22500 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Unnotched | 10 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 1.5 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | 120 - 180 sec | Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495 |
| Comparative Tracking Index | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
| Hot Wire Ignition, HWI | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | Min 150 mm/min | (+/- 0.125 inch); PLC Code 4; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 415 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 370 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 130 °C | UL 746B |
| UL RTI, Mechanical with Impact | 130 °C | UL 746B |
| UL RTI, Mechanical without Impact | 140 °C | UL 746B |
| Flammability, UL94 | V-0 | 0.03 in. |
| Flammability, UL94 | 7 | 0.118 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |