MatWeb, The Online Materials Database

SABIC Innovative Plastics VALOX EH7020 PBT (North America)


Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesMetricEnglishComments
Density1.49 g/cc0.0538 lb/in³ ASTM D 792
Linear Mold Shrinkage0.014 - 0.016 cm/cm0.014 - 0.016 in/in Flow, 60-125 mil; ASTM D 955
Linear Mold Shrinkage0.015 - 0.016 cm/cm0.015 - 0.016 in/in Flow, 125-180 mil; ASTM D 955
Linear Mold Shrinkage, Transverse0.013 - 0.014 cm/cm0.013 - 0.014 in/in 60-125 mil; ASTM D 955
Linear Mold Shrinkage, Transverse0.014 - 0.015 cm/cm0.014 - 0.015 in/in 125-180 mil; ASTM D 955

Mechanical Properties
Tensile Strength @ Break57.9 MPa8400 psi Type I, 0.2 in/min; ASTM D 638
Flexural Modulus4.14 GPa600 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Strength103 MPa15000 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Unnotched3.9 J/cm7.3 ft-lb/in 73F; ASTM D 4812
Izod Impact, Notched0.32 J/cm0.6 ft-lb/in 73F; ASTM D 256

Electrical Properties
Dielectric Constant2.92.9 1 MHz; ASTM D 150
Dielectric Constant3.13.1 50 Hz; ASTM D 150
Dielectric Strength16.9 kV/mm430 V/mil in oil, 125 mils; ASTM D 149
Dissipation Factor0.00390.0039 50 Hz; ASTM D 150
Dissipation Factor0.0140.014 1 MHz; ASTM D 150

Thermal Properties
CTE, linear 68°F55.8 µm/m-°C31 µin/in-°F Flow, -40F to 100F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)188 °C370 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)105 °C221 °F 0.250 inch, unannealed; ASTM D 648

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.