MatWeb, The Online Materials Database
SABIC Innovative Plastics VALOX EH7020 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Original Value | Comments |
|
Density | 1.49 g/cc | ASTM D 792 |
Linear Mold Shrinkage | 0.014 - 0.016 cm/cm | Flow, 60-125 mil; ASTM D 955 |
Linear Mold Shrinkage | 0.015 - 0.016 cm/cm | Flow, 125-180 mil; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.013 - 0.014 cm/cm | 60-125 mil; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.014 - 0.015 cm/cm | 125-180 mil; ASTM D 955 |
Mechanical Properties |
|
Tensile Strength @ Break | 8400 psi | Type I, 0.2 in/min; ASTM D 638 |
Flexural Modulus | 600000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 15000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 7.3 ft-lb/in | 73F; ASTM D 4812 |
Izod Impact, Notched | 0.6 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Dielectric Constant | 2.9 | 1 MHz; ASTM D 150 |
Dielectric Constant | 3.1 | 50 Hz; ASTM D 150 |
Dielectric Strength | 430 V/mil | in oil, 125 mils; ASTM D 149 |
Dissipation Factor | 0.0039 | 50 Hz; ASTM D 150 |
Dissipation Factor | 0.014 | 1 MHz; ASTM D 150 |
Thermal Properties |
|
CTE, linear 68°F | 31 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 370 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 221 °F | 0.250 inch, unannealed; ASTM D 648 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |