MatWeb, The Online Materials Database
SABIC Innovative Plastics VALOX FV608 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.35 g/cc | Molded Foam; ASTM D 792 |
| Density | 1.5 g/cc | ASTM D 792 |
| Water Absorption | 0.06 % | 24 hours @ 73F; ASTM D 570 |
| Water Absorption at Saturation | 0.13 % | Equilibrium, 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | Flow, 0.250 inch; ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 15700 psi | 0.250"; ASTM D 638 |
| Elongation at Break | 4.3 % | 0.250"; ASTM D 638 |
| Tensile Modulus | 1.195e+006 psi | 0.250"; ASTM D 638 |
| Flexural Modulus | 1e+006 psi | 0.250"; ASTM D 790 |
| Flexural Yield Strength | 23100 psi | 0.250"; ASTM D 790 |
| Izod Impact, Unnotched | 13 ft-lb/in | 73F; ASTM D 4812 |
| Falling Dart Impact | 12 ft-lb | 73F; GE Test |
Electrical Properties |
|
| Volume Resistivity | 3e+017 ohm-cm | ASTM D 257 |
| Surface Resistivity per Square | Min 1.1e+017 ohm | ASTM D 257 |
| Dielectric Constant | 2.81 | 1 MHz; ASTM D 150 |
| Dielectric Constant | 2.82 | 100 Hz; ASTM D 150 |
| Dielectric Strength | 335 V/mil | in air, 250 mils; ASTM D 149 |
| Dissipation Factor | 0.0012 | 100 Hz; ASTM D 150 |
| Dissipation Factor | 0.008 | 1 MHz; ASTM D 150 |
Thermal Properties |
|
| CTE, linear 68°F | 13 µin/in-°F | Flow, -40F to 200F; ASTM E 831 |
| Specific Heat Capacity | 0.28 BTU/lb-°F | ASTM C 351 |
| Deflection Temperature at 0.46 MPa (66 psi) | 405 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 295 °F | 0.250 inch, unannealed; ASTM D 648 |
| Oxygen Index | 20 % | ASTM D 2863 |
Descriptive Properties | |
| Foam Weight Reduction | 10% | Mechanical Properties Reported Herein (0.250") |
| Foam Weight Reduction | 10% | Impact Properties Reported Herein (0.250") |
| Foam Weight Reduction | 10% | Thermal Properties Reported Herein (0.250") |
| Foam Weight Reduction | 10% | Physical Properties Reported Herein (0.250") |
| Foam Weight Reduction | 20% | Electrical Properties Reported Herein (0.250") |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |