SABIC Innovative Plastics VALOX HR326HV PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.31 g/cc | ASTM D 792 |
| Water Absorption | 0.06 % | 24 hours @ 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.021 - 0.023 cm/cm | Flow, 0.125 inch; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.022 - 0.024 cm/cm | ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 8000 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 200 % | Type I, 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 350000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Strength | 12500 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Unnotched | 30 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 1 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Volume Resistivity | 2.5e+016 ohm-cm | ASTM D 257 |
| Dielectric Constant | 2.88 | 1 MHz; ASTM D 150 |
| Dielectric Constant | 2.9 | 50 Hz; ASTM D 150 |
| Dielectric Strength | 430 V/mil | in air, 125 mils; ASTM D 149 |
| Dissipation Factor | 0.001 | 50 Hz; ASTM D 150 |
| Dissipation Factor | 0.016 | 1 MHz; ASTM D 150 |
Thermal Properties |
|
| CTE, linear 68°F | 48 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
| CTE, linear 68°F | 66 µin/in-°F | Flow, -40F to 200F; ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 300 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 126 °F | 0.125 inch, unannealed; ASTM D 648 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |