SABIC Innovative Plastics VALOX 321 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.31 g/cc | 0.0473 lb/in³ | ASTM D 792 |
| Linear Mold Shrinkage | 0.009 - 0.016 cm/cm | 0.009 - 0.016 in/in | Flow, 30-90 mil; ASTM D 955 |
| Linear Mold Shrinkage | 0.015 - 0.023 cm/cm | 0.015 - 0.023 in/in | Flow, 90-180 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.01 - 0.017 cm/cm | 0.01 - 0.017 in/in | 30-90 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm | 0.016 - 0.024 in/in | 90-180 mil; ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 51.7 MPa | 7500 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 200 % | 200 % | Type I, 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 2.34 GPa | 340 ksi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Yield Strength | 82.7 MPa | 12000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Unnotched | 16 J/cm | 30 ft-lb/in | 73F; ASTM D 4812 |
| Gardner Impact | 40.7 J | 30 ft-lb | Modified Gardner, 73F; ASTM D 3029 |
| Izod Impact, Notched | 0.534 J/cm | 1 ft-lb/in | 73F; ASTM D 256 |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | 0.250 inch, unannealed; ASTM D 648 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |