| Physical Properties | Original Value | Comments |
|
| Density | 1.29 g/cc | ASTM D 792 |
| Water Absorption | 0.08 % | 24 hours @ 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | Flow, 30-90 mil; ASTM D 955 |
| Linear Mold Shrinkage | 0.017 - 0.023 cm/cm | Flow, 90-180 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.014 - 0.018 cm/cm | 30-90 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.017 - 0.022 cm/cm | 90-180 mil; ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 7000 psi | Type I, 2.0 in/min; ASTM D 638 |
| Elongation at Break | 200 % | Type I, 2.0 in/min; ASTM D 638 |
| Flexural Modulus | 320000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Yield Strength | 12000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Notched | 1.5 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Volume Resistivity | 1e+017 ohm-cm | ASTM D 257 |
| Dielectric Constant | 2.9 | 1 MHz; ASTM D 150 |
| Dielectric Strength | 406 V/mil | in air, 32 mils; ASTM D 149 |
| Dissipation Factor | 0.02 | 1 MHz; ASTM D 150 |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 305 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 130 °F | 0.250 inch, unannealed; ASTM D 648 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |