MatWeb, The Online Materials Database

SABIC Innovative Plastics VALOX 337 PBT (North America)


Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesOriginal ValueComments
Density1.22 g/cc ASTM D 792
Water Absorption0.1 % 24 hours @ 73F; ASTM D 570
Viscosity1.25e+006 cP Melt Viscosity; GE Test
Linear Mold Shrinkage0.024 - 0.027 cm/cm Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.024 - 0.027 cm/cm 0.125 inch; ASTM D 955
Melt Flow12.7 g/10 min 250C/5.0 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Yield5700 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Yield3.9 % Type I, 2.0 in/min; ASTM D 638
Flexural Modulus260000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength8200 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Unnotched60 ft-lb/in 73F; ASTM D 4812
Izod Impact, Notched, Low Temp15 ft-lb/in at -22F; ASTM D 256
Izod Impact, Notched, Low Temp60 ft-lb/in at -22F; ASTM D 4812
Izod Impact, Notched16.3 ft-lb/in 73F; ASTM D 256

Thermal Properties
Deflection Temperature at 0.46 MPa (66 psi)210 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)117 °F 0.250 inch, unannealed; ASTM D 648

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.