MatWeb, The Online Materials Database

SABIC Innovative Plastics VALOX 3706 PBT (North America)


Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their North American product line.

Physical PropertiesOriginal ValueComments
Density1.3 g/cc ASTM D 792
Linear Mold Shrinkage0.012 - 0.014 cm/cm Flow, 0.125 inch; ASTM D 955
Linear Mold Shrinkage, Transverse0.012 - 0.014 cm/cm 0.125 inch; ASTM D 955
Melt Flow23 g/10 min 260C/5.0 kgf; ASTM D 1238
Melt Flow23 g/10 min 266C/5.0 kgf; ASTM D 1238

Mechanical Properties
Tensile Strength @ Break5700 psi Type I, 2.0 in/min; ASTM D 638
Tensile Strength @ Yield7100 psi Type I, 2.0 in/min; ASTM D 638
Elongation at Break50 % Type I, 2.0 in/min; ASTM D 638
Elongation at Yield6 % Type I, 2.0 in/min; ASTM D 638
Tensile Modulus285000 psi 2.0 in/min; ASTM D 638
Flexural Modulus290000 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength11400 psi 0.05 in/min, 2" span; ASTM D 790
Gardner Impact @ 23°C440 in-lb Instrumented Impact Total Energy, 73°F; ASTM D 3763
Izod Impact, Notched12.5 ft-lb/in 73F; ASTM D 256

Electrical Properties
Arc Resistance60 - 120 sec Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495
Comparative Tracking Index250 - 400 V (+/- 0.125 inch); PLC Code 2; UL 746A
Hot Wire Ignition, HWI30 - 60 sec (+/- 0.125 inch); PLC Code 2; UL 746A
High Amp Arc Ignition, HAIMin 120 arcs Surface (+/- 0.125 inch); PLC Code 0; UL 746A
High Voltage Arc-Tracking Rate, HVTRMin 150 mm/min (+/- 0.125 inch); PLC Code 4; UL 746A

Thermal Properties
CTE, linear 68°F44 µin/in-°F Flow, -40F to 100F; ASTM E 831
CTE, linear 68°F, Transverse to Flow48 µin/in-°F from -40F to 100F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)260 °F 0.125 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)185 °F 0.125 inch, unannealed; ASTM D 648
Vicat Softening Point275 °F Rate B; ASTM D 1525
UL RTI, Electrical75 °C UL 746B
UL RTI, Mechanical with Impact75 °C UL 746B
UL RTI, Mechanical without Impact75 °C UL 746B
Flammability, UL94V-0 0.059 in.
Flammability, UL947 0.098 in.

Descriptive Properties
UL File Number, USAE121562 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.