Physical Properties | Metric | English | Comments |
|
Density | 1.58 g/cc | 0.0571 lb/in³ | ASTM D 792 |
Water Absorption | 0.06 % | 0.06 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | Flow, 60-125 mil; ASTM D 955 |
Linear Mold Shrinkage | 0.005 - 0.008 cm/cm | 0.005 - 0.008 in/in | Flow, 125-180 mil; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | 60-125 mil; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.006 - 0.009 cm/cm | 0.006 - 0.009 in/in | 125-180 mil; ASTM D 955 |
Mechanical Properties |
|
Hardness, Rockwell R | 119 | 119 | ASTM D 785 |
Tensile Strength @ Break | 117 MPa | 17000 psi | Type I, 0.2 in/min; ASTM D 638 |
Flexural Modulus | 7.58 GPa | 1100 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 186 MPa | 27000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 6.94 J/cm | 13 ft-lb/in | 73F; ASTM D 4812 |
Izod Impact, Notched | 0.641 J/cm | 1.2 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Volume Resistivity | Min 3.4e+016 ohm-cm | Min 3.4e+016 ohm-cm | ASTM D 257 |
Dielectric Constant | 3.7 | 3.7 | 1 MHz; ASTM D 150 |
Dielectric Constant | 3.8 | 3.8 | 100 Hz; ASTM D 150 |
Dielectric Strength | 19.3 kV/mm | 490 V/mil | in air, 125 mils; ASTM D 149 |
Dielectric Strength | 24 kV/mm | 610 V/mil | in oil, 62 mils; ASTM D 149 |
Dissipation Factor | 0.002 | 0.002 | 100 Hz; ASTM D 150 |
Dissipation Factor | 0.02 | 0.02 | 1 MHz; ASTM D 150 |
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | (+/- 0.125 inch); PLC Code 2; UL 746A |
High Amp Arc Ignition, HAI | Min 120 arcs | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | Min 150 mm/min | Min 5.91 in/min | (+/- 0.125 inch); PLC Code 4; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 25.2 µm/m-°C | 14 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear, 212°F (100°C) | 25.2 µm/m-°C | 14 µin/in-°F | Flow, 140F to 280F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 420 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | 0.125 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 204 °C | 400 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
Flammability, UL94 | V-0 | V-0 | 0.029 in. |
Flammability, UL94 | 7 | 7 | 0.079 in. |
Oxygen Index | 32 % | 32 % | ASTM D 2863 |
Descriptive Properties |
|
CSA File No. | LS88480 | |
UL File Number, USA | E121562 | |
UV-light, water exposure/immersion | F2 | UL746C |