Physical PropertiesOriginal ValueComments
Density1.53 g/cc ASTM D 792
Water Absorption0.06 % 24 hours @ 73F; ASTM D 570
Linear Mold Shrinkage0.003 - 0.005 cm/cm Flow, 60-125 mil; ASTM D 955
Linear Mold Shrinkage0.005 - 0.008 cm/cm Flow, 125-180 mil; ASTM D 955
Linear Mold Shrinkage, Transverse0.004 - 0.006 cm/cm 60-125 mil; ASTM D 955
Linear Mold Shrinkage, Transverse0.006 - 0.009 cm/cm 125-180 mil; ASTM D 955

Mechanical Properties
Hardness, Rockwell R118 ASTM D 785
Tensile Strength @ Break17300 psi Type I, 0.2 in/min; ASTM D 638
Flexural Modulus1.1e+006 psi 0.05 in/min, 2" span; ASTM D 790
Flexural Strength27500 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Unnotched15 ft-lb/in 73F; ASTM D 4812
Izod Impact, Notched1.6 ft-lb/in 73F; ASTM D 256

Electrical Properties
Volume ResistivityMin 3.2e+016 ohm-cm ASTM D 257
Dielectric Constant3.7 1 MHz; ASTM D 150
Dielectric Constant3.8 100 Hz; ASTM D 150
Dielectric Strength475 V/mil in air, 125 mils; ASTM D 149
Dielectric Strength630 V/mil in oil, 62 mils; ASTM D 149
Dissipation Factor0.002 100 Hz; ASTM D 150
Dissipation Factor0.02 1 MHz; ASTM D 150

Thermal Properties
CTE, linear 68°F14 µin/in-°F Flow, -40F to 100F; ASTM E 831
CTE, linear, 212°F (100°C)14 µin/in-°F Flow, 140F to 280F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)420 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)405 °F 0.250 inch, unannealed; ASTM D 648
Oxygen Index19 % ASTM D 2863

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.