MatWeb, The Online Materials Database
SABIC Innovative Plastics VALOX 430 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line. MatWeb has a separate entry for the European data sheet.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D 792 |
| Water Absorption | 0.05 % | 0.05 % | 24 hours @ 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | Flow, 60-125 mil; ASTM D 955 |
| Linear Mold Shrinkage | 0.005 - 0.008 cm/cm | 0.005 - 0.008 in/in | Flow, 125-180 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | 60-125 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.006 - 0.009 cm/cm | 0.006 - 0.009 in/in | 125-180 mil; ASTM D 955 |
Mechanical Properties |
|
| Hardness, Rockwell R | 125 | 125 | ASTM D 785 |
| Tensile Strength @ Break | 114 MPa | 16500 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 2 % | 2 % | Type I, 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 6.89 GPa | 1000 ksi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Strength | 172 MPa | 25000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Unnotched | 7.47 J/cm | 14 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 1.33 J/cm | 2.5 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten (+/- 0.125 inch); PLC Code 5; ASTM D 495 |
| Comparative Tracking Index | 400 - 600 V | 400 - 600 V | (+/- 0.125 inch); PLC Code 1; UL 746A |
| Hot Wire Ignition, HWI | Min 120 sec | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | Surface (+/- 0.125 inch); PLC Code 2; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 0 - 10 mm/min | 0 - 0.394 in/min | (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 222 °C | 431 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 204 °C | 400 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
| UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
| Flammability, UL94 | HB | HB | 0.058 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |