Physical PropertiesMetricEnglishComments
Density1.53 g/cc0.0553 lb/in³ ASTM D 792
Linear Mold Shrinkage0.003 - 0.005 cm/cm0.003 - 0.005 in/in Flow, 60-125 mil; ASTM D 955
Linear Mold Shrinkage0.005 - 0.008 cm/cm0.005 - 0.008 in/in Flow, 125-180 mil; ASTM D 955
Linear Mold Shrinkage, Transverse0.004 - 0.006 cm/cm0.004 - 0.006 in/in 60-125 mil; ASTM D 955
Linear Mold Shrinkage, Transverse0.006 - 0.009 cm/cm0.006 - 0.009 in/in 125-180 mil; ASTM D 955

Mechanical Properties
Tensile Strength @ Break110 MPa16000 psi Type I, 0.2 in/min; ASTM D 638
Flexural Modulus6.89 GPa1000 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength186 MPa27000 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Notched0.961 J/cm1.8 ft-lb/in 73F; ASTM D 256

Electrical Properties
Arc Resistance60 - 120 sec60 - 120 sec Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495
Comparative Tracking Index100 - 175 V100 - 175 V (+/- 0.125 inch); PLC Code 4; UL 746A
Hot Wire Ignition, HWI60 - 120 sec60 - 120 sec (+/- 0.125 inch); PLC Code 1; UL 746A
High Amp Arc Ignition, HAIMax 15 arcsMax 15 arcs Surface (+/- 0.125 inch); PLC Code 4; UL 746A
High Voltage Arc-Tracking Rate, HVTR25.4 - 80 mm/min1 - 3.15 in/min (+/- 0.125 inch); PLC Code 2; UL 746A

Thermal Properties
Deflection Temperature at 0.46 MPa (66 psi)204 °C400 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)160 °C320 °F 0.250 inch, unannealed; ASTM D 648
UL RTI, Electrical125 °C257 °F UL 746B
UL RTI, Mechanical with Impact110 °C230 °F UL 746B
UL RTI, Mechanical without Impact125 °C257 °F UL 746B
Flammability, UL94V-2V-2 0.058 in.

Descriptive Properties
UL File Number, USAE121562 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.