SABIC Innovative Plastics VALOX 553E PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
Physical Properties | Metric | English | Comments |
|
Density | 1.58 g/cc | 0.0571 lb/in³ | ASTM D 792 |
Water Absorption | 0.07 % | 0.07 % | 24 hours @ 73F; ASTM D 570 |
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | Flow, 60-125 mil; ASTM D 955 |
Linear Mold Shrinkage | 0.005 - 0.008 cm/cm | 0.005 - 0.008 in/in | Flow, 125-180 mil; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | 60-125 mil; ASTM D 955 |
Linear Mold Shrinkage, Transverse | 0.006 - 0.009 cm/cm | 0.006 - 0.009 in/in | 125-180 mil; ASTM D 955 |
Mechanical Properties |
|
Hardness, Rockwell R | 118 | 118 | ASTM D 785 |
Tensile Strength @ Break | 110 MPa | 16000 psi | Type I, 0.2 in/min; ASTM D 638 |
Flexural Modulus | 6.89 GPa | 1000 ksi | 0.05 in/min, 2" span; ASTM D 790 |
Flexural Strength | 179 MPa | 26000 psi | 0.05 in/min, 2" span; ASTM D 790 |
Izod Impact, Unnotched | 6.41 J/cm | 12 ft-lb/in | 73F; ASTM D 4812 |
Izod Impact, Notched | 0.854 J/cm | 1.6 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
Volume Resistivity | 4.3e+016 ohm-cm | 4.3e+016 ohm-cm | ASTM D 257 |
Dielectric Constant | 3.7 | 3.7 | 1 MHz; ASTM D 150 |
Dielectric Constant | 3.8 | 3.8 | 100 Hz; ASTM D 150 |
Dielectric Strength | 18.9 kV/mm | 480 V/mil | in air, 125 mils; ASTM D 149 |
Dielectric Strength | 25.6 kV/mm | 650 V/mil | in oil, 62 mils; ASTM D 149 |
Dissipation Factor | 0.002 | 0.002 | 100 Hz; ASTM D 150 |
Dissipation Factor | 0.02 | 0.02 | 1 MHz; ASTM D 150 |
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | (+/- 0.125 inch); PLC Code 3; UL 746A |
Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | (+/- 0.125 inch); PLC Code 1; UL 746A |
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | Surface (+/- 0.125 inch); PLC Code 3; UL 746A |
High Voltage Arc-Tracking Rate, HVTR | 80 - 150 mm/min | 3.15 - 5.91 in/min | (+/- 0.125 inch); PLC Code 3; UL 746A |
Thermal Properties |
|
CTE, linear 68°F | 21.6 µm/m-°C | 12 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
CTE, linear, 212°F (100°C) | 21.6 µm/m-°C | 12 µin/in-°F | Flow, 140F to 280F; ASTM E 831 |
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | 0.250 inch, unannealed; ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | 0.250 inch, unannealed; ASTM D 648 |
UL RTI, Electrical | 125 °C | 257 °F | UL 746B |
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
Flammability, UL94 | V-0 | V-0 | 0.034 in. |
Flammability, UL94 | 7 | 7 | 0.091 in. |
Oxygen Index | 37.1 % | 37.1 % | ASTM D 2863 |
Descriptive Properties | |
CSA File No. | LS88480 | |
UL File Number, USA | E121562 | |
UV-light, water exposure/immersion | F1 | UL746C |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|