SABIC Innovative Plastics VALOX 730 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Metric | English | Comments |
|
| Density | 1.55 g/cc | 0.056 lb/in³ | ASTM D 792 |
| Water Absorption | 0.08 % | 0.08 % | 24 hours @ 73F; ASTM D 570 |
| Linear Mold Shrinkage | 0.003 - 0.004 cm/cm | 0.003 - 0.004 in/in | Flow, 60-125 mil; ASTM D 955 |
| Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | Flow, 125-180 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.004 - 0.006 cm/cm | 0.004 - 0.006 in/in | 60-125 mil; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.006 - 0.008 cm/cm | 0.006 - 0.008 in/in | 125-180 mil; ASTM D 955 |
Mechanical Properties |
|
| Hardness, Rockwell R | 82 | 82 | ASTM D 785 |
| Tensile Strength @ Break | 65.5 MPa | 9500 psi | Type I, 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 6.21 GPa | 900 ksi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Yield Strength | 110 MPa | 16000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Unnotched | 3.74 J/cm | 7 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 0.534 J/cm | 1 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Volume Resistivity | 1.7e+015 ohm-cm | 1.7e+015 ohm-cm | ASTM D 257 |
| Dielectric Constant | 3.6 | 3.6 | 100 Hz; ASTM D 150 |
| Dielectric Constant | 3.6 | 3.6 | 1 MHz; ASTM D 150 |
| Dielectric Strength | 19.7 kV/mm | 500 V/mil | in air, 125 mils; ASTM D 149 |
| Dielectric Strength | 32.5 kV/mm | 825 V/mil | in oil, 62 mils; ASTM D 149 |
| Dissipation Factor | 0.002 | 0.002 | 100 Hz; ASTM D 150 |
| Dissipation Factor | 0.02 | 0.02 | 1 MHz; ASTM D 150 |
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten (+/- 0.125 inch); PLC Code 6; ASTM D 495 |
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | (+/- 0.125 inch); PLC Code 2; UL 746A |
| Hot Wire Ignition, HWI | Min 120 sec | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Amp Arc Ignition, HAI | Max 15 arcs | Max 15 arcs | Surface (+/- 0.125 inch); PLC Code 4; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 10 - 25.4 mm/min | 0.394 - 1 in/min | (+/- 0.125 inch); PLC Code 1; UL 746A |
Thermal Properties |
|
| CTE, linear 68°F | 30.6 µm/m-°C | 17 µin/in-°F | Flow, -40F to 100F; ASTM E 831 |
| CTE, linear, 212°F (100°C) | 36 µm/m-°C | 20 µin/in-°F | Flow, 140F to 280F; ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 171 °C | 340 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
| UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
| Flammability, UL94 | HB | HB | 0.058 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |