Physical PropertiesMetricEnglishComments
Density1.55 g/cc0.056 lb/in³ ASTM D 792
Water Absorption0.05 %0.05 % 24 hours @ 73F; ASTM D 570
Linear Mold Shrinkage0.004 - 0.006 cm/cm0.004 - 0.006 in/in Flow, 60-125 mil; ASTM D 955
Linear Mold Shrinkage0.006 - 0.009 cm/cm0.006 - 0.009 in/in Flow, 125-180 mil; ASTM D 955
Linear Mold Shrinkage, Transverse0.005 - 0.008 cm/cm0.005 - 0.008 in/in 60-125 mil; ASTM D 955
Linear Mold Shrinkage, Transverse0.008 - 0.011 cm/cm0.008 - 0.011 in/in 125-180 mil; ASTM D 955

Mechanical Properties
Hardness, Rockwell R113113 ASTM D 785
Tensile Strength @ Yield55.2 MPa8000 psi Type I, 2.0 in/min; ASTM D 638
Flexural Modulus3.45 GPa500 ksi 0.05 in/min, 2" span; ASTM D 790
Flexural Yield Strength103 MPa15000 psi 0.05 in/min, 2" span; ASTM D 790
Izod Impact, Unnotched10.7 J/cm20 ft-lb/in 73F; ASTM D 4812
Izod Impact, Notched0.534 J/cm1 ft-lb/in 73F; ASTM D 256

Electrical Properties
Volume Resistivity6.6e+015 ohm-cm6.6e+015 ohm-cm ASTM D 257
Dielectric Constant3.13.1 100 Hz; ASTM D 150
Dielectric Constant3.13.1 1 MHz; ASTM D 150
Dielectric Strength22.4 kV/mm570 V/mil in air, 125 mils; ASTM D 149
Dielectric Strength27.6 kV/mm700 V/mil in oil, 62 mils; ASTM D 149
Dissipation Factor0.0020.002 100 Hz; ASTM D 150
Dissipation Factor0.010.01 1 MHz; ASTM D 150

Thermal Properties
CTE, linear 68°F68.4 µm/m-°C38 µin/in-°F Flow, -40F to 100F; ASTM E 831
CTE, linear, 212°F (100°C)144 µm/m-°C80 µin/in-°F Flow, 140F to 280F; ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi)149 °C300 °F 0.250 inch, unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)76.7 °C170 °F 0.250 inch, unannealed; ASTM D 648

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.