MatWeb, The Online Materials Database
SABIC Innovative Plastics VALOX 771 PBT (North America)
Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.72 g/cc | ASTM D 792 |
| Linear Mold Shrinkage | 0.0065 - 0.0085 cm/cm | Flow; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.01 - 0.012 cm/cm | ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength @ Break | 10500 psi | Type I, 0.2 in/min; ASTM D 638 |
| Elongation at Break | 2.3 % | Type I, 0.2 in/min; ASTM D 638 |
| Flexural Modulus | 850000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Flexural Strength | 16000 psi | 0.05 in/min, 2" span; ASTM D 790 |
| Izod Impact, Unnotched | 7 ft-lb/in | 73F; ASTM D 4812 |
| Izod Impact, Notched | 0.8 ft-lb/in | 73F; ASTM D 256 |
Electrical Properties |
|
| Arc Resistance | 180 - 240 sec | Tungsten (+/- 0.125 inch); PLC Code 4; ASTM D 495 |
| Comparative Tracking Index | Min 600 V | (+/- 0.125 inch); PLC Code 0; UL 746A |
| Hot Wire Ignition, HWI | Min 120 sec | (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Amp Arc Ignition, HAI | Min 120 arcs | Surface (+/- 0.125 inch); PLC Code 0; UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 0 - 10 mm/min | (+/- 0.125 inch); PLC Code 0; UL 746A |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 423 °F | 0.250 inch, unannealed; ASTM D 648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 385 °F | 0.250 inch, unannealed; ASTM D 648 |
| UL RTI, Electrical | 140 °C | UL 746B |
| UL RTI, Mechanical with Impact | 125 °C | UL 746B |
| UL RTI, Mechanical without Impact | 140 °C | UL 746B |
| Flammability, UL94 | V-2 | 0.024 in. |
| Flammability, UL94 | V-0 | 0.03 in. |
| Flammability, UL94 | 7 | 0.079 in. |
Descriptive Properties | |
| UL File Number, USA | E121562 | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from