SABIC Innovative Plastics CYCOLOY C1100 ABS + Polycarbonate (Europe)


Subcategory: ABS Polymer; Polycarbonate; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line.

Physical PropertiesMetricEnglishComments
Density1.12 g/cc0.0405 lb/in³ ASTM D 792
Density1.12 g/cc0.0405 lb/in³ ISO 1183
Moisture Absorption at Equilibrium0.2 %0.2 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.6 %0.6 % 23C; ISO 62
Viscosity213000 cP213000 cP Melt Viscosity (MV), 260 C, 1500 1/sec; DIN 54811
Linear Mold Shrinkage0.005 - 0.007 cm/cm0.005 - 0.007 in/in Flow; ASTM D 955
Melt Flow14 g/10 min14 g/10 min cm3/10min; Melt Volume Rate, MVR at 260C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, Rockwell R117117 ISO 2039/2
Hardness, H358/3096 MPa13900 psi ISO 2039/1
Tensile Strength, Ultimate40 MPa5800 psi 5 mm/min; ISO 527
Tensile Strength, Ultimate45 MPa6530 psi 50 mm/min; ISO 527
Tensile Strength, Yield45 MPa6530 psi 5 mm/min; ISO 527
Tensile Strength, Yield55 MPa7980 psi 50 mm/min; ISO 527
Elongation at BreakMin 50 %Min 50 % 50 mm/min; ISO 527
Elongation at Break80 %80 % 5 mm/min; ISO 527
Elongation at Yield4 %4 % 5 mm/min; ISO 527
Elongation at Yield4 %4 % 50 mm/min; ISO 527
Tensile Modulus2.4 GPa348 ksi 1 mm/min; ISO 527
Flexural Modulus2.3 GPa334 ksi 2 mm/min; ISO 178
Flexural Yield Strength80 MPa11600 psi 2 mm/min; ISO 178
Izod Impact, Notched (ISO)41 kJ/m²19.5 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched (ISO)NBNB 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)NBNB 80*10*4 -30 C; ISO 180/ 1U
Izod Impact, Notched, Low Temp (ISO)17 kJ/m²8.09 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1A
Charpy Impact, Notched, Low Temp2 J/cm²9.52 ft-lb/in² at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Charpy Impact, Notched4.2 J/cm²20 ft-lb/in² 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles7979 CS-17, 1 kg; GE Test

Electrical Properties
Volume ResistivityMin 1e+015 ohm-cmMin 1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohmMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant2.72.7 1 MHz; IEC 60250
Dielectric Constant2.82.8 50 Hz; IEC 60250
Dielectric Strength17 kV/mm432 kV/in in oil, 3.2 mm; IEC 60243-1
Dielectric Strength25 kV/mm635 kV/in in oil, 1.6 mm; IEC 60243-1
Dielectric Strength35 kV/mm889 kV/in in oil, 0.8 mm; IEC 60243-1
Dissipation Factor0.0020.002 50 Hz; IEC 60250
Dissipation Factor0.0070.007 1 MHz; IEC 60250
Comparative Tracking Index200 V200 V Stand. Black; IEC 60112/3rd
Comparative Tracking Index250 V250 V IEC 60112/3rd
Comparative Tracking Index250 V250 V M; IEC 60112/3rd
Comparative Tracking Index250 V250 V Electr Grey; IEC 60112/3rd

Thermal Properties
CTE, linear 20°C80 µm/m-°C44.4 µin/in-°F 23C-60C, flow; ISO 11359-2
CTE, linear 20°C Transverse to Flow80 µm/m-°C44.4 µin/in-°F 23C-60C; ISO 11359-2
Thermal Conductivity0.2 W/m-K1.39 BTU-in/hr-ft²-°F ISO 8302
Hot Ball Pressure TestMax 110 °CMax 230 °F IEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi)120 °C248 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)100 °C212 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point120 °C248 °F B/50; ISO 306
Vicat Softening Point123 °C253 °F B/120; ISO 306
UL RTI, Electrical60 °C140 °F UL 746B
UL RTI, Mechanical with Impact60 °C140 °F UL 746B
UL RTI, Mechanical without Impact60 °C140 °F UL 746B
Flammability, UL94HBHB 1.5 mm
Glow Wire Test650 °C1200 °F Passes at 1 mm; IEC 60695-2-1
Glow Wire Test750 °C1380 °F Passes at 1 mm; EDF HN60S02

Descriptive Properties
Ball Pressure Test, 75 C +/- 2 CPASSES IEC 60035-1

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.