MatWeb, The Online Materials Database

SABIC Innovative Plastics ULTEM CRS5311 Polyetherimide (Europe)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

Physical PropertiesOriginal ValueComments
Density1.52 g/cc ASTM D 792
Density1.52 g/cc ISO 1183
Moisture Absorption at Equilibrium0.15 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.9 % 23C; ISO 62
Linear Mold Shrinkage0.002 - 0.004 cm/cm Flow; ASTM D 955
Melt Flow7 g/10 min cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, H358/30165 MPa ISO 2039/1
Tensile Strength, Ultimate160 MPa 5 mm/min; ISO 527
Elongation at Break2 % 5 mm/min; ISO 527
Tensile Modulus10 GPa 1 mm/min; ISO 527
Flexural Modulus8.2 GPa 2 mm/min; ISO 178
Flexural Strength210 MPa 2 mm/min; ISO 178
Compressive Modulus8.3 GPa DIN 53454
Izod Impact, Unnotched (ISO)35 kJ/m² 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)35 kJ/m² 80*10*4 -30 C; ISO 180/ 1U

Electrical Properties
Volume Resistivity1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant3.1 1 MHz; IEC 60250
Dielectric Constant3.2 50 Hz; IEC 60250
Dielectric Strength18 kV/mm in oil, 3.2 mm; IEC 60243-1
Dissipation Factor0.002 50 Hz; IEC 60250
Dissipation Factor0.003 1 MHz; IEC 60250
Comparative Tracking Index100 V M; IEC 60112/3rd
Comparative Tracking Index150 V IEC 60112/3rd

Thermal Properties
CTE, linear 100°C20 µm/m-°C 23C-150C, flow; ISO 11359-2
CTE, linear 100°C70 µm/m-°C 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.33 W/m-K ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)215 °C HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)215 °C HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point220 °C B/120; ISO 306
Vicat Softening Point228 °C A/50; ISO 306
UL RTI, Electrical105 °C UL 746B
UL RTI, Mechanical with Impact105 °C UL 746B
UL RTI, Mechanical without Impact105 °C UL 746B
Flammability, UL94V-0 1.5 mm
Flammability, UL947 94-1.5 mm
Flammability Test1 mm; IEC Needle Flame Test, 10 s , passes at; IEC 60695-2-2
Glow Wire Test960 °C Passes at 3.2 mm; EDF HN60S02
Glow Wire Test960 °C Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.