SABIC Innovative Plastics ULTEM 1110F Polyetherimide (Europe)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

Physical PropertiesMetricEnglishComments
Density1.37 g/cc0.0495 lb/in³ ASTM D 792
Density1.37 g/cc0.0495 lb/in³ ISO 1183
Moisture Absorption at Equilibrium0.65 %0.65 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation1.2 %1.2 % 23C; ISO 62
Linear Mold Shrinkage0.004 - 0.006 cm/cm0.004 - 0.006 in/in Flow; ASTM D 955
Melt Flow12 g/10 min12 g/10 min cm3/10min; Melt Volume Rate, MVR at 340C/5.0 kg; ISO 1133
Melt Flow21 g/10 min21 g/10 min cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, H358/30145 MPa21000 psi ISO 2039/1
Tensile Strength, Ultimate80 MPa11600 psi 50 mm/min; ISO 527
Tensile Strength, Yield110 MPa16000 psi 50 mm/min; ISO 527
Elongation at Break10 %10 % 50 mm/min; ISO 527
Elongation at Yield6 %6 % 50 mm/min; ISO 527
Tensile Modulus3.5 GPa508 ksi 1 mm/min; ISO 527
Flexural Modulus3.3 GPa479 ksi 2 mm/min; ISO 178
Flexural Yield Strength140 MPa20300 psi 2 mm/min; ISO 178
Izod Impact, Notched (ISO)4 kJ/m²1.9 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Notched, Low Temp (ISO)4 kJ/m²1.9 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1A
Taber Abrasion, mg/1000 Cycles1010 CS-17, 1 kg; GE Test

Electrical Properties
Volume Resistivity1e+015 ohm-cm1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohmMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant3.53.5 50 Hz; IEC 60250
Dielectric Strength17.2 kV/mm437 kV/in in oil, 3.2 mm; IEC 60243-1
Dissipation Factor0.00160.0016 50 Hz; IEC 60250
Comparative Tracking Index125 V125 V M; IEC 60112/3rd
Comparative Tracking Index175 V175 V IEC 60112/3rd

Thermal Properties
CTE, linear 100°C50 µm/m-°C27.8 µin/in-°F 23C-150C, flow; ISO 11359-2
CTE, linear 100°C50 µm/m-°C27.8 µin/in-°F 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.26 W/m-K1.8 BTU-in/hr-ft²-°F ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)200 °C392 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)185 °C365 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point200 °C392 °F B/50; ISO 306
Vicat Softening Point205 °C401 °F B/120; ISO 306
Vicat Softening Point210 °C410 °F A/50; ISO 306
Flammability, UL94V-0V-0 0.74 mm; UL 94 by GE
Oxygen Index47 %47 % ISO 4589
Glow Wire Test960 °C1760 °F Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.