Physical PropertiesOriginal ValueComments
Density1.43 g/cc ASTM D 792
Density1.43 g/cc ISO 1183
Linear Mold Shrinkage0.003 - 0.005 cm/cm Flow; ASTM D 955

Mechanical Properties
Tensile Strength, Ultimate75 MPa 5 mm/min; ISO 527
Elongation at Break8 % 5 mm/min; ISO 527
Tensile Modulus4.5 GPa 1 mm/min; ISO 527
Flexural Yield Strength135 MPa 2 mm/min; ISO 178
Compressive Modulus4.5 GPa ASTM D 695
Izod Impact, Unnotched (ISO)30 kJ/m² 80*10*4 +23 C; ISO 180/ 1U

Thermal Properties
Thermal Conductivity0.28 W/m-K ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)202 °C HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)189 °C HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point211 °C B/120; ISO 306
Vicat Softening Point220 °C Rate B; ASTM D 1525
UL RTI, Electrical170 °C UL 746B
UL RTI, Mechanical with Impact170 °C UL 746B
UL RTI, Mechanical without Impact170 °C UL 746B
Flammability, UL94V-0 0.41 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.