MatWeb, The Online Materials Database
SABIC Innovative Plastics ULTEM 2212R Polyetherimide (Europe)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.
| Physical Properties | Original Value | Comments |
|
| Density | 1.43 g/cc | ASTM D 792 |
| Density | 1.43 g/cc | ISO 1183 |
| Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | Flow; ASTM D 955 |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 75 MPa | 5 mm/min; ISO 527 |
| Elongation at Break | 8 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 4.5 GPa | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 135 MPa | 2 mm/min; ISO 178 |
| Compressive Modulus | 4.5 GPa | ASTM D 695 |
| Izod Impact, Unnotched (ISO) | 30 kJ/m² | 80*10*4 +23 C; ISO 180/ 1U |
Thermal Properties |
|
| Thermal Conductivity | 0.28 W/m-K | ISO 8302 |
| Deflection Temperature at 0.46 MPa (66 psi) | 202 °C | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 189 °C | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| Vicat Softening Point | 211 °C | B/120; ISO 306 |
| Vicat Softening Point | 220 °C | Rate B; ASTM D 1525 |
| UL RTI, Electrical | 170 °C | UL 746B |
| UL RTI, Mechanical with Impact | 170 °C | UL 746B |
| UL RTI, Mechanical without Impact | 170 °C | UL 746B |
| Flammability, UL94 | V-0 | 0.41 mm |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |