SABIC Innovative Plastics ULTEM 2310R Polyetherimide (Europe)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

Physical PropertiesMetricEnglishComments
Density1.51 g/cc0.0546 lb/in³ ASTM D 792
Density1.51 g/cc0.0546 lb/in³ ISO 1183
Water Absorption0.18 %0.18 % 24 hours; ASTM D 570
Moisture Absorption at Equilibrium0.5 %0.5 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.9 %0.9 % 23C; ISO 62
Linear Mold Shrinkage0.002 - 0.004 cm/cm0.002 - 0.004 in/in Flow; ASTM D 955

Mechanical Properties
Hardness, Rockwell M114114 ISO 2039/2
Hardness, H358/30165 MPa23900 psi ISO 2039/1
Tensile Strength, Ultimate160 MPa23200 psi ASTM D 638
Tensile Strength, Ultimate165 MPa23900 psi 5 mm/min; ISO 527
Elongation at Break2 %2 % 5 mm/min; ISO 527
Elongation at Break3 %3 % ASTM D 638
Tensile Modulus9 GPa1310 ksi DIN 53457
Tensile Modulus9.5 GPa1380 ksi 1 mm/min; ISO 527
Flexural Modulus8.5 GPa1230 ksi 2 mm/min; ISO 178
Flexural Modulus9 GPa1310 ksi DIN 53457
Flexural Strength225 MPa32600 psi 2 mm/min; ISO 178
Ultimate Compressive Strength175 MPa25400 psi ASTM D 695
Compressive Modulus7.5 GPa1090 ksi DIN 53454
Shear Strength100 MPa14500 psi ASTM D 732
Izod Impact, Notched1 J/cm1.87 ft-lb/in 23 C; ASTM D 256
Izod Impact, Unnotched4.3 J/cm8.06 ft-lb/in 23 C; ASTM D 4812
Izod Impact, Unnotched (ISO)40 kJ/m²19 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)40 kJ/m²19 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1U
Charpy Impact Unnotched4 J/cm²19 ft-lb/in² 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Unnotched Low Temp4 J/cm²19 ft-lb/in² at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Notched1 J/cm²4.76 ft-lb/in² 23 C; ISO 179/2C
Taber Abrasion, mg/1000 Cycles2020 CS-17, 1 kg; GE Test

Electrical Properties
Volume Resistivity1e+015 ohm-cm1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohmMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant3.33.3 50 Hz; IEC 60250
Dielectric Constant3.43.4 1 MHz; IEC 60250
Dielectric Strength15 kV/mm381 kV/in in oil, 3.2 mm; IEC 60243-1
Dielectric Strength26 kV/mm660 kV/in in oil, 1.6 mm; IEC 60243-1
Dielectric Strength35 kV/mm889 kV/in in oil, 0.8 mm; IEC 60243-1
Dissipation Factor0.00150.0015 1 kHz; IEC 60250
Dissipation Factor0.00160.0016 50 Hz; IEC 60250
Dissipation Factor0.00230.0023 1 MHz; IEC 60250
Dissipation Factor0.00530.0053 2450 MHz; IEC 60250
Arc Resistance85 sec85 sec Tungsten; ASTM D 495

Thermal Properties
CTE, linear 100°C20 µm/m-°C11.1 µin/in-°F 23C-150C, flow; ISO 11359-2
CTE, linear 100°C60 µm/m-°C33.3 µin/in-°F 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.3 W/m-K2.08 BTU-in/hr-ft²-°F ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)212 °C414 °F ASTM D 648
Deflection Temperature at 0.46 MPa (66 psi)215 °C419 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)210 °C410 °F ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)210 °C410 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point213 °C415 °F B/50; ISO 306
Vicat Softening Point220 °C428 °F B/120; ISO 306
Vicat Softening Point225 °C437 °F A/50; ISO 306
Vicat Softening Point228 °C442 °F Rate B; ASTM D 1525
UL RTI, Electrical180 °C356 °F UL 746B
UL RTI, Mechanical with Impact170 °C338 °F UL 746B
UL RTI, Mechanical without Impact180 °C356 °F UL 746B
Flammability, UL94V-0V-0 0.25 mm
Flammability, UL9477 94-1.2 mm
Oxygen Index48 %48 % ISO 4589
Glow Wire Test960 °C1760 °F Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
MPa; Hardness, H961/30290 DIN 53456

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.