MatWeb, The Online Materials Database

SABIC Innovative Plastics ULTEM 2410R Polyetherimide (Europe)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

Physical PropertiesOriginal ValueComments
Density1.61 g/cc ASTM D 792
Density1.61 g/cc ISO 1183
Water Absorption0.12 % 24 hours; ASTM D 570
Moisture Absorption at Equilibrium0.4 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.8 % 23C; ISO 62
Linear Mold Shrinkage0.001 - 0.003 cm/cm Flow; ASTM D 955
Melt Flow7 g/10 min cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, Rockwell M125 ISO 2039/2
Hardness, H358/30170 MPa ISO 2039/1
Tensile Strength, Ultimate180 MPa 5 mm/min; ISO 527
Tensile Strength, Yield186 MPa ASTM D 638
Elongation at Break2 % 5 mm/min; ISO 527
Elongation at Break2.5 % ASTM D 638
Tensile Modulus11.5 GPa 1 mm/min; ISO 527
Tensile Modulus11.7 GPa DIN 53457
Flexural Modulus10 GPa 2 mm/min; ISO 178
Flexural Modulus11.7 GPa DIN 53457
Flexural Strength240 MPa 2 mm/min; ISO 178
Ultimate Compressive Strength200 MPa ASTM D 695
Compressive Modulus10 GPa DIN 53454
Shear Strength103 MPa ASTM D 732
Izod Impact, Notched1.05 J/cm 23 C; ASTM D 256
Izod Impact, Unnotched4.3 J/cm 23 C; ASTM D 4812
Izod Impact, Unnotched (ISO)35 kJ/m² 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)35 kJ/m² 80*10*4 -30 C; ISO 180/ 1U
Charpy Impact Unnotched4 J/cm² 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Unnotched Low Temp4 J/cm² at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Taber Abrasion, mg/1000 Cycles20 CS-17, 1 kg; GE Test

Electrical Properties
Volume Resistivity1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant3.1 1 MHz; IEC 60250
Dielectric Constant3.5 50 Hz; IEC 60250
Dielectric Strength16 kV/mm in oil, 3.2 mm; IEC 60243-1
Dielectric Strength26 kV/mm in oil, 1.6 mm; IEC 60243-1
Dielectric Strength35 kV/mm in oil, 0.8 mm; IEC 60243-1
Dissipation Factor0.0019 1 MHz; IEC 60250
Dissipation Factor0.002 1 kHz; IEC 60250
Dissipation Factor0.0025 50 Hz; IEC 60250

Thermal Properties
CTE, linear 100°C15 µm/m-°C 23C-150C, flow; ISO 11359-2
CTE, linear 100°C45 µm/m-°C 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.33 W/m-K ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)215 °C HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 0.46 MPa (66 psi)216 °C ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)210 °C HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Deflection Temperature at 1.8 MPa (264 psi)213 °C ASTM D 648
Vicat Softening Point217 °C B/50; ISO 306
Vicat Softening Point225 °C B/120; ISO 306
Vicat Softening Point230 °C A/50; ISO 306
Vicat Softening Point234 °C Rate B; ASTM D 1525
UL RTI, Electrical105 °C UL 746B
UL RTI, Mechanical with Impact105 °C UL 746B
UL RTI, Mechanical without Impact105 °C UL 746B
Flammability, UL94V-0 0.25 mm
Flammability, UL947 94-1.5 mm
NBS Smoke Density1 Flaming, Ds 4 min; ASTM E 662
NBS Smoke Density20 Flaming, Dmax 20 min; ASTM E 662
Oxygen Index48 % ISO 4589
Glow Wire Test960 °C Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.