MatWeb, The Online Materials Database

SABIC Innovative Plastics ULTEM 6000 Polyetherimide (Europe)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line.

Physical PropertiesOriginal ValueComments
Density1.3 g/cc ASTM D 792
Density1.3 g/cc ISO 1183
Water Absorption0.28 % 24 hours; ASTM D 570
Moisture Absorption at Equilibrium0.8 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation1 % 23C; ISO 62
Linear Mold Shrinkage0.004 - 0.006 cm/cm Flow; ASTM D 955
Melt Flow7 g/10 min cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, H358/30160 MPa ISO 2039/1
Tensile Strength, Ultimate95 MPa 50 mm/min; ISO 527
Tensile Strength, Yield103 MPa ASTM D 638
Elongation at Break30 % ASTM D 638
Elongation at Break4 % 50 mm/min; ISO 527
Elongation at Yield8 % ASTM D 638
Tensile Modulus3 GPa DIN 53457
Tensile Modulus3.3 GPa 1 mm/min; ISO 527
Flexural Modulus3 GPa DIN 53457
Flexural Modulus3.1 GPa 2 mm/min; ISO 178
Flexural Yield Strength140 MPa 2 mm/min; ISO 178
Flexural Yield Strength145 MPa DIN 53452
Ultimate Compressive Strength140 MPa ASTM D 695
Shear Strength100 MPa ASTM D 732
Izod Impact, Notched0.4 J/cm 23 C; ASTM D 256
Izod Impact, Notched (ISO)5 kJ/m² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched13 J/cm 23 C; ASTM D 4812
Izod Impact, Notched, Low Temp (ISO)5 kJ/m² 80*10*4 -30 C; ISO 180/ 1A

Electrical Properties
Volume Resistivity1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant3.2 50 Hz; IEC 60250
Dielectric Strength18.6 kV/mm in oil, 3.2 mm; IEC 60243-1
Dielectric Strength29 kV/mm in oil, 1.6 mm; IEC 60243-1
Dissipation Factor0.0015 50 Hz; IEC 60250
Arc Resistance127 sec Tungsten; ASTM D 495
Comparative Tracking Index100 V M; IEC 60112/3rd
Comparative Tracking Index150 V IEC 60112/3rd

Thermal Properties
CTE, linear 100°C45 µm/m-°C 23C-150C, flow; ISO 11359-2
CTE, linear 100°C45 µm/m-°C 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.26 W/m-K ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)210 °C HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 0.46 MPa (66 psi)221 °C ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi)200 °C HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Deflection Temperature at 1.8 MPa (264 psi)215 °C ASTM D 648
Vicat Softening Point220 °C B/120; ISO 306
Vicat Softening Point222 °C B/50; ISO 306
UL RTI, Electrical105 °C UL 746B
UL RTI, Mechanical with Impact105 °C UL 746B
UL RTI, Mechanical without Impact105 °C UL 746B
Flammability, UL94V-0 1.5 mm
Flammability Test3.2 mm; IEC Needle Flame Test, 10 s , passes at; IEC 60695-2-2
NBS Smoke Density5 Flaming, Ds 4 min; ASTM E 662
Oxygen Index47 % ISO 4589
Glow Wire Test960 °C Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1
Needle Flame Test, 3.2 mm, Burn Time sPASSES IEC 60695-2-2

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.