Physical Properties | Metric | English | Comments |
|
Density | 1.43 g/cc | 0.0517 lb/in³ | ASTM D 792 |
Water Absorption | 0.22 % | 0.22 % | 24 hours; ASTM D 570 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 145 MPa | 21000 psi | ASTM D 638 |
Elongation at Break | 4 % | 4 % | ASTM D 638 |
Tensile Modulus | 6.9 GPa | 1000 ksi | DIN 53457 |
Flexural Modulus | 6.5 GPa | 943 ksi | DIN 53457 |
Flexural Strength | 210 MPa | 30500 psi | DIN 53452 |
Ultimate Compressive Strength | 170 MPa | 24700 psi | ASTM D 695 |
Shear Strength | 95 MPa | 13800 psi | ASTM D 732 |
Izod Impact, Notched | 0.8 J/cm | 1.5 ft-lb/in | 23 C; ASTM D 256 |
Izod Impact, Unnotched | 4 J/cm | 7.49 ft-lb/in | 23 C; ASTM D 4812 |
Electrical Properties |
|
Volume Resistivity | 1e+015 ohm-cm | 1e+015 ohm-cm | IEC 60093 |
Dielectric Strength | 23 kV/mm | 584 kV/in | in oil, 1.6 mm; IEC 60243-1 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 225 °C | 437 °F | ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 223 °C | 433 °F | ASTM D 648 |
Vicat Softening Point | 243 °C | 469 °F | Rate B; ASTM D 1525 |
Flammability, UL94 | V-0 | V-0 | 1.5 mm |
Flammability Test | 3.2 | 3.2 | mm; IEC Needle Flame Test, 10 s , passes at; IEC 60695-2-2 |
NBS Smoke Density | 4 | 4 | Flaming, Ds 4 min; ASTM E 662 |
Oxygen Index | 44 % | 44 % | ISO 4589 |
Descriptive Properties | |
Needle Flame Test, 3.2 mm, Burn Time s | PASSES | IEC 60695-2-2 |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|