SABIC Innovative Plastics ULTEM 6200 Polyetherimide (Europe)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Information provided by GE Plastics for their European product line.
Physical Properties | Original Value | Comments |
|
Density | 1.43 g/cc | ASTM D 792 |
Water Absorption | 0.22 % | 24 hours; ASTM D 570 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 145 MPa | ASTM D 638 |
Elongation at Break | 4 % | ASTM D 638 |
Tensile Modulus | 6.9 GPa | DIN 53457 |
Flexural Modulus | 6.5 GPa | DIN 53457 |
Flexural Strength | 210 MPa | DIN 53452 |
Ultimate Compressive Strength | 170 MPa | ASTM D 695 |
Shear Strength | 95 MPa | ASTM D 732 |
Izod Impact, Notched | 0.8 J/cm | 23 C; ASTM D 256 |
Izod Impact, Unnotched | 4 J/cm | 23 C; ASTM D 4812 |
Electrical Properties |
|
Volume Resistivity | 1e+015 ohm-cm | IEC 60093 |
Dielectric Strength | 23 kV/mm | in oil, 1.6 mm; IEC 60243-1 |
Thermal Properties |
|
Deflection Temperature at 0.46 MPa (66 psi) | 225 °C | ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 223 °C | ASTM D 648 |
Vicat Softening Point | 243 °C | Rate B; ASTM D 1525 |
Flammability, UL94 | V-0 | 1.5 mm |
Flammability Test | 3.2 | mm; IEC Needle Flame Test, 10 s , passes at; IEC 60695-2-2 |
NBS Smoke Density | 4 | Flaming, Ds 4 min; ASTM E 662 |
Oxygen Index | 44 % | ISO 4589 |
Descriptive Properties | |
Needle Flame Test, 3.2 mm, Burn Time s | PASSES | IEC 60695-2-2 |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|