SABIC Innovative Plastics ULTEM 9076 Polyetherimide (Europe)


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line. This product is also a part of their North American product line.

Physical PropertiesOriginal ValueComments
Density1.3 g/cc ISO 1183
Density1.32 g/cc ASTM D 792
Moisture Absorption at Equilibrium0.7 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation1.25 % 23C; ISO 62
Linear Mold Shrinkage0.006 - 0.008 cm/cm Flow; ASTM D 955
Melt Flow22 g/10 min cm3/10min; Melt Volume Rate, MVR at 360C/5.0 kg; ISO 1133

Mechanical Properties
Hardness, H358/30145 MPa ISO 2039/1
Tensile Strength, Ultimate70 MPa 50 mm/min; ISO 527
Tensile Strength, Yield95 MPa 50 mm/min; ISO 527
Elongation at Break50 % 50 mm/min; ISO 527
Elongation at Yield6 % 50 mm/min; ISO 527
Tensile Modulus3 GPa 1 mm/min; ISO 527
Flexural Modulus3 GPa 2 mm/min; ISO 178
Flexural Yield Strength135 MPa 2 mm/min; ISO 178
Izod Impact, Notched (ISO)6 kJ/m² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Notched, Low Temp (ISO)6 kJ/m² 80*10*4 -30 C; ISO 180/ 1A
Charpy Impact, Notched, Low Temp0.6 J/cm² at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Charpy Impact, Notched0.6 J/cm² 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA

Electrical Properties
Volume ResistivityMin 1e+015 ohm-cm IEC 60093
Surface Resistivity per SquareMin 1e+015 ohm ROA; IEC 60093
Dielectric Constant2.8 1 MHz; IEC 60250
Dielectric Constant2.9 50 Hz; IEC 60250
Dielectric Strength18 kV/mm in oil, 3.2 mm; IEC 60243-1
Dissipation Factor0.005 1 MHz; IEC 60250
Comparative Tracking Index150 V IEC 60112/3rd

Thermal Properties
CTE, linear 100°C55 µm/m-°C 23C-150C, flow; ISO 11359-2
CTE, linear 100°C55 µm/m-°C 23C-150C, cross flow; ISO 11359-2
Thermal Conductivity0.26 W/m-K ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)195 °C HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)175 °C HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point200 °C B/50; ISO 306
Vicat Softening Point200 °C B/120; ISO 306
Vicat Softening Point210 °C A/50; ISO 306
Oxygen Index50 % ISO 4589
Glow Wire Test960 °C Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.