SABIC Innovative Plastics VALOX DR48V PBT (Europe)


Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Information provided by GE Plastics for their European product line.

Physical PropertiesMetricEnglishComments
Density1.51 g/cc0.0546 lb/in³ ASTM D 792
Density1.51 g/cc0.0546 lb/in³ ISO 1183
Moisture Absorption at Equilibrium0.07 %0.07 % (23 C / 50% RH) 1L; ISO 15512
Water Absorption at Saturation0.17 %0.17 % 23C; ISO 62
Linear Mold Shrinkage0.005 - 0.008 cm/cm0.005 - 0.008 in/in Flow; ASTM D 955
Linear Mold Shrinkage, Transverse0.006 - 0.009 cm/cm0.006 - 0.009 in/in ASTM D 955
Melt Flow12 g/10 min12 g/10 min cm3/10min; Melt Volume Rate, MVR at 250C/2.16 kg; ISO 1133

Mechanical Properties
Hardness, Rockwell R118118 ISO 2039/2
Tensile Strength, Ultimate110 MPa16000 psi 5 mm/min; ISO 527
Elongation at Break2 %2 % 5 mm/min; ISO 527
Tensile Modulus6.5 GPa943 ksi 1 mm/min; ISO 527
Flexural Modulus5.5 GPa798 ksi 2 mm/min; ISO 178
Flexural Strength160 MPa23200 psi 2 mm/min; ISO 178
Ultimate Compressive Strength103 MPa14900 psi ASTM D 695
Shear Strength55 MPa7980 psi ASTM D 732
Izod Impact, Notched (ISO)5 kJ/m²2.38 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1A
Izod Impact, Unnotched (ISO)50 kJ/m²23.8 ft-lb/in² 80*10*4 +23 C; ISO 180/ 1U
Izod Impact, Unnotched Low Temp (ISO)50 kJ/m²23.8 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1U
Izod Impact, Notched, Low Temp (ISO)5 kJ/m²2.38 ft-lb/in² 80*10*4 -30 C; ISO 180/ 1A
Charpy Impact Unnotched5.5 J/cm²26.2 ft-lb/in² 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.4 J/cm²1.9 ft-lb/in² at -30C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Charpy Impact, Unnotched Low Temp5 J/cm²23.8 ft-lb/in² at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU
Charpy Impact, Notched0.5 J/cm²2.38 ft-lb/in² 23C, V-notch Edgew 80*10*4 sp=62; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles1616 CS-17, 1 kg; GE Test

Electrical Properties
Volume ResistivityMin 1e+013 ohm-cmMin 1e+013 ohm-cm IEC 60093
Surface Resistivity per Square1.8e+014 ohm1.8e+014 ohm ROA; IEC 60093
Dielectric Constant3.43.4 1 MHz; IEC 60250
Dielectric Constant3.63.6 50 Hz; IEC 60250
Dielectric Strength19 kV/mm483 kV/in Short time, 1.0 mm; IEC 60243-1
Dielectric Strength19 kV/mm483 kV/in in oil, 3.2 mm; IEC 60243-1
Dissipation Factor0.0020.002 50 Hz; IEC 60250
Dissipation Factor0.020.02 1 MHz; IEC 60250
Comparative Tracking Index150 V150 V M; IEC 60112/3rd
Comparative Tracking Index175 V175 V IEC 60112/3rd

Thermal Properties
CTE, linear 20°C35 µm/m-°C19.4 µin/in-°F 23C-80C, flow; ISO 11359-2
CTE, linear 20°C Transverse to Flow95 µm/m-°C52.8 µin/in-°F 23C-80C; ISO 11359-2
Thermal Conductivity0.19 W/m-K1.32 BTU-in/hr-ft²-°F ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)215 °C419 °F HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi)185 °C365 °F HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point185 °C365 °F B/50; ISO 306
Vicat Softening Point185 °C365 °F B/120; ISO 306
Vicat Softening Point213 °C415 °F Rate B; ASTM D 1525
Flammability, UL94V-0V-0 0.89 mm
Flammability, UL9477 94-3 mm
Oxygen Index31 %31 % ISO 4589
Glow Wire Test960 °C1760 °F Passes at 3.2 mm; IEC 60695-2-1

Descriptive Properties
Ball Pressure Test, 125 C +/- 2 CPASSES IEC 60035-1

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.