| Physical Properties | Original Value | Comments |
|
| Density | 1.42 g/cc | ASTM D 792 |
| Density | 1.42 g/cc | ISO 1183 |
| Moisture Absorption at Equilibrium | 0.06 % | (23 C / 50% RH) 1L; ISO 15512 |
| Water Absorption at Saturation | 0.1 % | 23C; ISO 62 |
| Linear Mold Shrinkage | 0.003 - 0.008 cm/cm | Flow; ASTM D 955 |
| Linear Mold Shrinkage, Transverse | 0.006 - 0.009 cm/cm | ASTM D 955 |
| Melt Flow | 14 g/10 min | cm3/10min; Melt Volume Rate, MVR at 250C/2.16 kg; ISO 1133 |
Mechanical Properties |
|
| Hardness, H358/30 | 95 MPa | ISO 2039/1 |
| Tensile Strength, Ultimate | 105 MPa | 5 mm/min; ISO 527 |
| Elongation at Break | 2 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 7.2 GPa | 1 mm/min; ISO 527 |
| Flexural Modulus | 6.2 GPa | 2 mm/min; ISO 178 |
| Flexural Strength | 160 MPa | 2 mm/min; ISO 178 |
| Flexural Yield Strength | 155 MPa | 2 mm/min; ISO 178 |
| Izod Impact, Unnotched (ISO) | 30 kJ/m² | 80*10*4 +23 C; ISO 180/ 1U |
| Izod Impact, Unnotched Low Temp (ISO) | 30 kJ/m² | 80*10*4 -30 C; ISO 180/ 1U |
| Charpy Impact Unnotched | 3.5 J/cm² | 23C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
| Charpy Impact, Unnotched Low Temp | 3.5 J/cm² | at -30C, Unnotch Edgew 80*10*4 sp=62; ISO 179/1eU |
Electrical Properties |
|
| Volume Resistivity | Min 1e+015 ohm-cm | IEC 60093 |
| Surface Resistivity per Square | Min 1e+015 ohm | ROA; IEC 60093 |
| Dielectric Constant | 3.2 | 1 MHz; IEC 60250 |
| Dielectric Constant | 3.3 | 50 Hz; IEC 60250 |
| Dielectric Constant | 3.4 | 100 Hz; IEC 60250 |
| Dielectric Strength | 18 kV/mm | in oil, 3.2 mm; IEC 60243-1 |
| Dissipation Factor | 0.001 | 50 Hz; IEC 60250 |
| Dissipation Factor | 0.013 | 1 MHz; IEC 60250 |
| Comparative Tracking Index | 125 V | M; IEC 60112/3rd |
| Comparative Tracking Index | 200 V | IEC 60112/3rd |
Thermal Properties |
|
| CTE, linear 20°C | 30 µm/m-°C | 23C-60C, flow; ISO 11359-2 |
| CTE, linear 20°C Transverse to Flow | 60 µm/m-°C | 23C-60C; ISO 11359-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 170 °C | HDT/Ae, 1.82 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| Vicat Softening Point | 165 °C | B/50; ISO 306 |
| Vicat Softening Point | 170 °C | B/120; ISO 306 |
| Glow Wire Test | 850 °C | Passes at 3.2 mm; IEC 60695-2-1 |
Descriptive Properties |
|
| Ball Pressure Test, 125 C +/- 2 C | PASSES | IEC 60035-1 |