SABIC Innovative Plastics ULTEM® CRS5112 Polyetherimide, 10% Glass Filled, Injection Grade


Subcategory: Filled/Reinforced Thermoplastic; Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.

Physical PropertiesMetricEnglishComments
Density1.36 g/cc0.0491 lb/in³ ASTM D792
Melt Flow9 g/10 min9 g/10 min 335°C/6.6kg; ASTM D1238

Mechanical Properties
Tensile Strength, Ultimate82 MPa11900 psi ASTM D638
Elongation at Break16 %16 % ASTM D638
Flexural Modulus3.9 GPa566 ksi 6.4 mm sample; ASTM D790
Flexural Yield Strength152 MPa22000 psi ASTM D790
Izod Impact, Notched0.4 J/cm0.749 ft-lb/in 3.2 mm sample; ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)207 °C405 °F 6.4 mm (0.25 in.) sample; ASTM D648

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.