Physical Properties | Metric | English | Comments |
|
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.003 - 0.005 cm/cm | 0.003 - 0.005 in/in | 3.2 mm sample |
Melt Flow | 2.6 g/10 min | 2.6 g/10 min | 295°C/6.6kg; ASTM D1238 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 93 MPa | 13500 psi | ASTM D638 |
Elongation at Break | 85 % | 85 % | ASTM D638 |
Modulus of Elasticity | 2.9 GPa | 421 ksi | ASTM D638 |
Flexural Modulus | 3.1 GPa | 450 ksi | 3.2 mm sample; ASTM D790 |
Izod Impact, Notched | 0.9 J/cm | 1.69 ft-lb/in | 3.2 mm sample; ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 190 °C | 374 °F | 6.4 mm (0.25 in.) sample; ASTM D648 |
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
UL RTI, Mechanical with Impact | 115 °C | 239 °F | UL 746B |
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
Flammability, UL94 | V-0 | V-0 | 0.8 mm |
Processing Properties |
|
Processing Temperature | 332 - 354 °C | 630 - 669 °F | Suggested injection molding melt temperature |
Mold Temperature | 93 - 135 °C | 199 - 275 °F | |
Drying Temperature | 135 °C | 275 °F | |
Dry Time | 4 - 6 hour | 4 - 6 hour | 12 hr Max. |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|