MatWeb, The Online Materials Database

SABIC Innovative Plastics ULTEM® MD133 Polyetherimide+PPO, 30% Glass Filled, Injection Grade


Subcategory: Filled/Reinforced Thermoplastic; Polyetherimide; Polymer; Polyphenylene Ether/PPO; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Data for 3.2 mm (1/8 in) samples unless otherwise noted. Data provided by GE Plastics.

Physical PropertiesMetricEnglishComments
Density1.43 g/cc0.0517 lb/in³ ASTM D792
Water Absorption0.18 %0.18 % 24 hrs; 20°C; ASTM D570
Melt Flow5.1 g/10 min5.1 g/10 min 335°C/6.6kg; ASTM D1238

Mechanical Properties
Tensile Strength, Ultimate131 MPa19000 psi ASTM D638
Modulus of Elasticity9.6 GPa1390 ksi ASTM D638
Flexural Modulus9 GPa1310 ksi 6.4 mm sample; ASTM D790
Izod Impact, Notched0.6 J/cm1.12 ft-lb/in 3.2 mm sample; ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)208 °C406 °F 6.4 mm (0.25 in.) sample; ASTM D648

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.