SABIC Innovative Plastics ULTEM® 1010S PEI, Unfilled


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.

Physical PropertiesMetricEnglishComments
Density1.27 g/cc0.0459 lb/in³ ASTM D792
Water Absorption0.25 %0.25 % 24 hrs at 23°C; ASTM D570
Linear Mold Shrinkage0.005 - 0.007 cm/cm0.005 - 0.007 in/in at 3.2 mm.

Mechanical Properties
Tensile Strength, Ultimate105 MPa15200 psi ASTM D638
Elongation at Break60 %60 % ASTM D638
Tensile Modulus2.963 GPa430 ksi ASTM D638
Flexural Modulus3.307 GPa480 ksi ASTM D790
Flexural Yield Strength152 MPa22000 psi ASTM D790
Izod Impact, Notched0.33 J/cm0.618 ft-lb/in 23°C (73.4°F)

Electrical Properties
Electrical Resistivity1e+017 ohm-cm1e+017 ohm-cm ASTM D257

Thermal Properties
Deflection Temperature at 0.46 MPa (66 psi)207 °C405 °F ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)197 °C387 °F ASTM D648
Vicat Softening Point218 °C424 °F ASTM D1525

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.